Surface Treatment
Magnet Surface Treatment Services
Sintered NdFeB corrodes without protection. The finish you pick decides whether a magnet survives a humid warehouse, a coastal install or a wash-down line, and it changes the dimensions of the part.
How a coating is applied
Four stages from cleaned metal to an inspected finish.
Pretreatment
The machined surface is cleaned and activated so the finish bonds to sound metal, not to grinding residue.
Plating or coating
The agreed finish is applied to the specified thickness, with edge coverage checked on the sample.
Post-treatment
Nickel-copper-nickel parts are baked in a pressure-cooker cycle to drive out hydrogen and prevent the blistering that appears weeks later.
Inspection
Thickness, adhesion and corrosion performance are checked to the coating specification; salt-spray and PCT results are recorded per lot.
The Menu
Coatings and where each one fits
Seven finishes cover the duty range we see.
| Coating | Where it fits |
|---|---|
| Nickel-copper-nickel (NiCuNi) | The industrial default. Typically 10 to 20 µm, bright metallic, specified to 96 h pressure-cooker and 48 to 72 h neutral salt spray in our standard specification. |
| Zinc | Economical bright finish for indoor and dry duty. Thinner and softer than NiCuNi; not the choice for salt air. |
| Epoxy | Black or grey, typically thicker than plating. The choice for wash-down and salt-water duty, and electrically insulating. |
| Parylene | Thin, conformal, vacuum-deposited. A moisture barrier where the controlling dimension must stay tight. |
| Tin | Solderable surface, used where the magnet is joined by solder in an assembly. |
| Gold | Conductive and corrosion-resistant, for sensor and instrument duty where contact resistance matters. |
| Phosphating | Matt conversion base for paint or for adhesive bonding, where a plating layer would defeat the bond. |
Choosing by environment
The environment picks the coating; everything else is preference. Two rules cover most decisions: bare zinc does not belong in salt air, and NdFeB under a breached coating corrodes from beneath the plating long before the coating itself fails.
- Indoor, dry: zinc or NiCuNi
- Humid or coastal: epoxy, or NiCuNi with a seal step
- High temperature: NiCuNi, which holds to the highest temperature of the plated finishes
- Tight dimensions: parylene, the thinnest of the menu
- Solder joint: tin
- Adhesive bonding: phosphating or epoxy, so the adhesive bonds to the coating rather than to plating it cannot wet

Dimensions
How coating changes the part
Plating adds material, so the pre-plate size is adjusted to hold your final dimension.
| Controlling dimension | Tell us which dimension controls and we machine the pre-plate size so the finished part lands on it |
|---|---|
| Holes and threads | Plating follows the geometry; masked features stay uncoated where the assembly calls for it |
| Edge coverage | Checked on the pre-production sample; thin edges are the first place a thin coating fails |
| Post-plate bake | NiCuNi goes through a PCT cycle to prevent hydrogen blistering in service |
| Colour | Epoxy is available in black and grey; plating finishes are metallic unless sealed |
Documents available on request
Coating documents we share during a project — request the current version from our team.
Go Deeper
Related reading
- Magnet surface treatment — what each finish does to corrosion resistance
- Neodymium coating options — the plating menu compared side by side
- Epoxy versus nickel coating — choosing between the two most common finishes
- Zinc versus nickel coating — cost against corrosion resistance
- Neodymium corrosion and protection — why a breached coating is worse than no coating
Buyer Questions
Surface Treatment FAQs
Which coating do you recommend outdoors?
Epoxy, or NiCuNi with a seal step. Bare zinc corrodes quickly in salt air, and NdFeB under a breached coating corrodes from beneath the plating.
Does the coating change the dimensions?
Yes. Plating adds thickness, so we adjust the pre-plate size to hold your final dimension. Tell us which dimension controls and we machine to it.
Can you match a specific coating or colour?
Send a sample or a colour reference. We match to the closest standard finish and confirm it on a pre-production sample before the run.
Is NiCuNi baked after plating?
Yes. NiCuNi parts go through a pressure-cooker bake to drive out hydrogen and prevent the blistering that shows up weeks after delivery.
Can parts be delivered uncoated?
Uncoated blanks are supplied for customers who plate or bond in-house, packed with corrosion protection and a shelf-life note. Tell us at the quotation stage.
Send us the requirement
Tell us the application, the duty and the quantity. You get a specification, a schedule and a quote in writing.
Request a quote