Sintered neodymium magnets are often specified only by their magnetic numbers - remanence, coercivity and energy product - yet the mechanical and thermal physical properties decide how the part is machined, mounted and cooled. This article collects the standard sintered NdFeB physical properties and explains what each one means on the bench and in the field.
Density and mass
Sintered NdFeB has a density of 7.40-7.70 g/cm³, which places it among the heavier engineering ceramics and metals. For handheld devices and rotating parts, that mass feeds directly into weight budgets and rotational inertia. Because the density is high and predictable, it also makes a useful cross-check: a finished magnet that is markedly lighter than its volume implies may be porous or poorly sintered.
Hardness and machinability
The Vickers hardness of 500-700 HV puts sintered NdFeB in the same league as tool steels and hardened ceramics. It is hard enough to take a fine edge yet brittle, so it cannot be machined like metal. Shaping is done by grinding with diamond tooling, not by cutting or drilling, and the part must be supported to avoid chipping. Designers should specify near-net shapes and leave only light grinding allowance rather than expecting post-sinter machining of complex features.
Strength: compressive, tensile and bending
The material is strong in compression (1000-1100 MPa) but weak in tension (80-90 MPa) and modest in bending (150-400 MPa). That asymmetry is the reason neodymium magnets fail by cracking rather than yielding. In service this means the magnet should be loaded in compression or held in a housing that prevents tensile and bending stress - never relied upon as a structural member spanning a gap. Mounting designs that clamp the magnet between soft facings and avoid point loads will outlast those that bolt or cantilever it.
Young's modulus and stiffness
A Young's modulus of 150-200 GPa gives sintered NdFeB a stiffness comparable to aluminium alloys, so it will not flex appreciably under its own weight but will transmit vibration and shock. Combined with the low tensile strength, this stiffness means impact energy is absorbed by cracking rather than deforming, reinforcing the case for cushioned, compressive mounting.
Thermal behaviour
Several thermal figures matter for design. The Curie temperature of 310-380℃ is the point at which the ferromagnetic order collapses; it is a material limit, not a working temperature, and the practical operating ceiling for standard grades is far lower at 80℃. The temperature coefficient of remanence is -0.085 to -0.125 %/K, meaning the field falls by roughly a tenth of a percent per kelvin of warming, while the intrinsic coercivity coefficient of -0.42 to -0.80 %/K shows coercivity falling faster with heat - the reason higher-temperature series exist. Thermal conductivity of 6-10 W/(m·K) is low, so a magnet heats and cools slowly and any local hot spot lingers.
Thermal expansion is anisotropic
Because the grains are aligned during pressing, the coefficient of thermal expansion differs with direction: about -2 to 0 ×10⁻⁵/K perpendicular to the magnetisation axis and 4-9 ×10⁻⁵/K parallel to it. Designers should expect the magnet to grow mainly along its magnetisation direction when warmed and to behave nearly neutrally across it. In tightly fitted assemblies this anisotropy can induce stress if the housing expands differently, so allow for it in interference-fit designs.
Electrical and recoil properties
The electrical resistivity of 1.2-1.6 µΩ·m is low enough that eddy currents can be a concern in rapidly changing fields, which is why thin laminations or segmented poles are sometimes used in high-speed rotors. The recoil permeability of about 1.05 means the magnet behaves almost like a permanent source with little rebound in its working line, a useful simplification when modelling the magnetic circuit.
A design checklist
When you take a sintered NdFeB part from a drawing to a product, keep four physical facts in view: it is hard and brittle so it grinds, not cuts; it is strong in compression but weak in tension so it mounts in compression; it warms and cools slowly so plan for heat sinking; and it expands mainly along its axis so allow for anisotropy in tight fits. Ticking these off prevents most field failures that have nothing to do with the magnetic grade.
What the physical properties do not tell you
The table captures the bulk behaviour of sintered NdFeB, but it is not the whole story. It is a reference for design and selection, not an acceptance criterion for a finished part, and real components also depend on coating integrity, edge condition and how the magnet is mounted. Two magnets with identical physical-property bands can fail very differently in the field if one is poorly coated or point-loaded.
Comparing NdFeB to other materials
Against ferrite, NdFeB is far denser and stronger magnetically but more brittle and corrosion-prone. Against the rare-earth cousins, its physical character is similar - hard, brittle, anisotropic - while its temperature behaviour differs sharply. The physical properties therefore reinforce a simple rule: choose the family for magnetics and temperature first, then design the mount and finish around these mechanical facts.
Mounting that respects the strength profile
Given 1000-1100 MPa in compression but only 80-90 MPa in tension, the safe design loads the magnet between soft steel facings and never lets it span a gap or take a bending load. Adhesive retention works well when the bond area is large and the load is compressive; mechanical clamps should seat on the faces, not the edges.
Heat and the working limit
The 310-380℃ Curie point is a material ceiling, not a use temperature; the practical limit for standard grades is 80℃ and for the temperature-rated series up to 230℃. The negative temperature coefficient of remanence means the field also sags with warmth, so thermal design and magnetic design are the same conversation.
Why these numbers matter to buyers
You do not need to memorise the table, but you should know the implications: the magnet is heavy, so weight budget it; it is brittle, so mount it in compression; it warms and cools slowly, so plan heat paths; and it expands along its axis, so allow for fit. Those four points turn the physical-property table into practical design rules.
Frequently asked questions
Can neodymium magnets be drilled or milled? Not practically. At 500-700 HV they are ground with diamond tooling; cutting or drilling tends to crack them, so near-net shaping is preferred.
Why do they crack instead of bend? High compressive but low tensile and bending strength means impact and tensile loads are relieved by fracture rather than yielding.
Does the Curie temperature tell me the working limit? No. The Curie point of 310-380℃ is where magnetism vanishes; the usable operating limit for standard grades is 80℃, with higher tiers reaching 230℃.
How much does the field drop with temperature? Remanence falls about 0.085-0.125 %/K, so a 50 K rise trims the field by roughly 4-6 percent before any coercivity effects.
Why does the expansion differ by direction? Grain alignment during pressing makes the material anisotropic, so it grows about 4-9 ×10⁻⁵/K along the magnetisation axis and near zero across it.