Sintered permanent magnets are among the hardest materials in a typical assembly and among the most fragile. A magnet that survives a 700-newton pull force can be chipped by dropping it onto a steel bench, and the fracture that results is sudden, complete and usually permanent. Understanding where breakage comes from is the difference between a part that survives assembly and one that generates complaints.
The material is brittle by nature
NdFeB, ferrite, SmCo and alnico are all sintered or cast solids with essentially no ductility. They do not bend, they do not yield, and they do not blunt an impact the way a steel part does. NdFeB has a compressive strength in the region of 1000 to 1100 megapascals but a tensile strength a fraction of that, which means it performs well under squeezing loads and badly under any load that tries to pull it apart, such as a bending moment on an overhanging section.
Where the damage actually comes from
- Impact between magnets: two free magnets attracting each other collide at closing speed and chip their edges or corners. This is the single most common cause of damage in handling.
- Drops onto steel: a magnet dropped onto a bench bounces, and the corner that hits first takes the load.
- Thermal shock: a hot magnet quenched, or a cold magnet plunged into warm water, cracks from differential contraction.
- Grinding damage: too aggressive a cut burns the surface, leaves residual tensile stress, and starts a crack that appears later.
- Design factors: sharp internal corners, thin webs, unsupported overhangs and knife edges concentrate stress at exactly the places the material is weakest.
What can be specified
Breakage is managed with three levers. First, geometry: generous corner radii, no knife edges, and minimum wall thicknesses for the grade and size. Second, edge treatment: a controlled edge break or chamfer turns a fragile 90-degree corner into a robust one at almost no cost. Third, packaging: parts separated by foam or blister trays, so they cannot reach each other in transit. All three are drawing decisions, and all three are cheaper than a field-failure investigation.
Acceptance criteria
Not every chip is a defect. The industry practice is to define an acceptance envelope on the drawing: a maximum chip size and count per face, a maximum depth, and exclusion zones where no chip is acceptable at all, typically the pole faces and any locating surface. Without that definition, "chipped magnet" becomes a matter of opinion between buyer and supplier, and the disagreement is unresolvable after the fact.
Handling guidance for assembly lines
Wear eye protection, because a cracking magnet can throw fragments. Keep magnets apart until the moment of assembly, using spacers or keeper plates. Never let two free magnets approach each other uncontrolled. Warm parts to room temperature before assembly if they have come from a cold store, and do not bond onto a hot substrate without checking the adhesive's temperature limit. A line that follows those rules sees a small fraction of the breakage rate of one that does not.
Frequently asked questions
Is a chipped magnet still safe to use?Mechanically, if the chip is outside a critical zone and the part still meets its dimensional envelope, yes. Magnetically, a chip removes material and changes the flux slightly, so re-measure rather than assume.
Why did my magnets arrive broken?Almost always transit impact. Ask the supplier how the parts were packed; if they were loose in a box, the packaging spec needs fixing, not the parts.
Can a cracked magnet be repaired?No. There is no practical adhesive joint that restores the magnetic circuit or the strength of the parent material.
Does a thicker coating make a magnet tougher?An epoxy layer adds impact tolerance and protects the edges, which is why epoxy is common on parts destined for rough handling. It does not make the magnet itself less brittle.
Designing a part for rough handling? Send the drawing and the assembly method and we will suggest the geometry, edge treatment and packing that fit.