EDUCATION

What Is Intrinsic Coercivity (Hcj)? Why It Beats Plain Coercivity | YUECI KEJI

Intrinsic coercivity is the number behind every M, H, SH, UH, EH and AH suffix in the magnet world. It is also the number most buyers have never had explained to them.

Intrinsic coercivity, written Hcj, is the strength of an opposing magnetic field needed to permanently erase a magnet's magnetization. It is the single number that separates a base grade from a temperature-rated one, and it is the reason a magnet specified for a hot motor costs more than the same shape in a base grade.

Coercivity versus intrinsic coercivity

There are two coercivity numbers on a datasheet, and they are not the same. Normal coercivity, Hcb, is the opposing field needed to bring the magnet's delivered flux density to zero: past this point the magnet produces nothing usable. Intrinsic coercivity, Hcj, is the opposing field needed to erase the magnetization itself: past this point the magnet is scrap. Hcj is always the larger of the two, often by a factor of close to two in NdFeB, and it is the one that tells you how much abuse the magnet can survive.

Why the suffixes exist

Every temperature-class suffix in the NdFeB range is a statement about intrinsic coercivity. A plain N52 is built for room temperature and demagnetizes easily. Adding dysprosium or terbium, or using grain boundary diffusion to concentrate them at the grain boundaries, raises Hcj and with it the temperature the magnet can work at. That is the whole story behind M for around 100 degrees, H for around 120, SH for around 150, UH for around 180, EH for around 200 and AH for around 230 degrees of continuous working temperature.

What Hcj protects against

Three things, all of them "an opposing field appeared". A motor under overload drives current that produces a field opposed to the magnet's own. A generator under short circuit does the same. An assembly where two magnets are forced into an unfavorable orientation can do it mechanically. In each case the question is not whether the opposing field exceeded Hcb but whether it exceeded Hcj, because only the second one is permanent damage.

Why a high-Hcj magnet can read weaker

This surprises buyers who compare grades on a gaussmeter. The techniques that raise intrinsic coercivity, particularly heavy rare-earth additions, tend to reduce remanence slightly. A 52SH magnet often reads lower on the surface than a plain 52 of identical geometry, because it is engineered to hold its field under attack rather than to deliver the highest possible field in ideal conditions. The right comparison is at temperature, under the opposing field your application actually produces, not on the bench at room temperature.

Units and typical values

Intrinsic coercivity is quoted in kiloampere per metre (kA/m) or kilo-oersted (kOe), with one kOe equal to about 79.6 kA/m. Base NdFeB grades sit in the region of 12 kOe, H classes around 17 kOe, SH around 20 kOe, and the higher classes move up from there. Values below roughly 12 kOe in NdFeB are a signal that the grade was not designed to survive any real opposing field.

What to specify

If your application runs hot or sees current spikes, specify the temperature class or a minimum Hcj rather than a remanence alone, and tell the supplier the worst-case opposing field and temperature together. If the application is a benign, room-temperature holding duty, a base grade is the economical choice and a high-Hcj grade is money spent on a risk you do not have. The grade selection guide sets out the decision in full.

Frequently asked questions

Is higher Hcj always better? It is always safer, but it usually costs remanence and money. The right level is the one that covers your actual temperature and opposing-field exposure with a margin, not the highest available.

Can I tell the class from the grade number alone? No. The number gives the energy product; the letter gives the temperature class and therefore the intrinsic coercivity. N52 and N52SH are different materials engineered for different duties.

Does ferrite have the same distinction? Yes in principle, but ferrite's coercivity is high relative to its remanence in a way that makes it naturally resistant, which is one reason it persists in hot motor duties.

What happens if I under-specify Hcj? Nothing, until the day a hot start, an overload or a fault condition pushes the magnet past its limit. Then the machine quietly loses torque and nobody can find the cause, because the magnet looks unchanged.

Choosing a temperature class for a motor or generator? Send us the duty and the field conditions and we will recommend a grade with the margin you need.