Technology

Hydrogen Decrepitation and Jet Milling: Preparing NdFeB Powder for Pressing | YUECI KEJI

Between the alloy flakes and the pressed blank sit two powder-preparation stages that quietly determine whether the magnet will meet its grade: hydrogen decrepitation and jet milling.

Between the alloy flakes and the pressed blank sit two powder-preparation stages that quietly determine whether the magnet will meet its grade: hydrogen decrepitation and jet milling.

Why the alloy must be powdered

Pressing needs a powder that flows into the die, packs evenly and orients in the aligning field. Cast alloy is far too coarse for that, so it is reduced to a controlled particle-size distribution first.

Hydrogen decrepitation

Hydrogen is absorbed into the alloy flakes, which makes them expand and crack along grain boundaries until they break into a coarse powder. The step is gentle on the material and leaves the composition intact, which is why it replaced mechanical crushing as the standard route. YUECI KEJI holds a utility-model patent on fine-powder filtration for the hydrogen-decrepitation furnace.

Jet milling

The coarse powder is then milled in a high-velocity gas jet, where particles break by collision rather than by contact with a grinding medium. That keeps contamination out and produces the fine, narrow size distribution pressing needs. YUECI KEJI's patents cover jet-mill nozzles and airflow-based separation of magnetic material.

Upstream and downstream neighbours

Before decrepitation, the alloy flakes are produced by vacuum strip casting and may pass through coarse crushing — the company holds a patent on resonance coarse-crushing equipment for NdFeB raw material and one on rare-earth batching. After milling, the powder goes straight to the aligning press.

Why particle size matters to the buyer

Particle size sets how the powder packs and orients, which feeds both density and anisotropy. A well-milled powder gives a more uniform blank, and a uniform blank gives a magnet whose measured results sit closer to the middle of the grade band.

Controlling the powder, controlling the magnet

Oxygen pickup during milling is the main risk, because surface oxide degrades both the pressed blank and the coating that follows. Dry handling, controlled storage and short milling-to-pressing intervals are the standard countermeasures, and they are equipment problems rather than recipe problems.

How the stages connect

Strip casting sets the microstructure the hydrogen step will exploit; decrepitation sets the particle structure jet milling will refine; milling sets what the press can orient. A weakness at any one of the three carries through to the finished magnet.

Frequently asked questions

Why hydrogen and not just crushing? Hydrogen cracks the alloy along its own grain boundaries, so the powder inherits a fine, uniform structure that mechanical crushing would smear and contaminate.

What particle size does pressing need? A fine, narrow distribution — typically a few micrometres. Too coarse and the blank is porous; too fine and the powder oxidises and flows poorly.

Is the powder oxygen-sensitive? Yes. Powder handling is kept dry and controlled, which is why filtration and storage equipment appear in the patent list.

Can powder be stored before pressing? Only briefly and under controlled conditions; it normally goes to the press soon after milling.

If your project needs a specific grade, geometry or magnetic result, Request a quote and share the drawing or the duty conditions.